Inconel 718 is a widely used superalloy that is relatively economical however has good mechanical characteristics. Inconel 718 is heat processed at different temperatures. The grain sizes were measured on both samples by using Light Optical Microscope. The mechanical test results show the damage of tensile strength and hardness while enhancement of creep life with … Continue reading Effect of grain size on mechanical properties of Inconel 718