EverForge Specialty Alloys Co., Ltd.

Industrial specifications of superalloys

Corrosion Resistant Alloys

Hastelloy B2

Wire: ASME SB-335, A5.14 ERNiMo-7, ASME SFA 5.11(ENiMo-7) AWS A5.11 (ENiMo-7)Sheet: ASME SB-333, ASTM B333Plate :ASME SB-333

Pipe: ASME SB-622, ASME SB-619, ASME SB-626, ASTM B622, CLASS I or II

Rod: ASME SB-335, ASME SFA 5.14(ENiMo-7)

Hastelloy C22

Wire: ASTM B574, ISO 9723, ISO 9724, DIN 17752, DIN  17753, AWS A5.14 ERNiCrMo-10, AWS A5.11 ENiCrMo-10Sheet. Strip, Plate: ASTM B 575; ASTM B 906 & ASME SB 575; ASME SB 906, ASME Code Case 2226, ASME Code Case N-621, ISO 6208, DIN 17750Pipe, Tube : ASTM B 619; ASTM B 775 & ASME SB 619; ASME SB 775, ASTM B 622; ASTM B 829 & ASME SB 622; ASME SB 829, ASTM B 626; ASTM B 751 & ASME SB 626; ASME SB 751, ASME Code Case 2226, ASME Code Case N-621, ISO 6207, DIN 17751

Rod, Bar: ASTM B 462, ASTM B 574 & ASME SB 574, , ASME Code Case N-621, ISO 9723, ISO 9724, DIN 17752, ASME Code Case 2226, ), DIN 17753

Others: ASTM B 366 & ASME SB-366

Hastelloy C276

Wire : ASTM B574,  ASME SB 574, ISO 9724. ISO 9724, DIN 17752. DIN 17753, DIN 17754 VdTüV 400/12.98, Filler Metal C276, AWS A5.14 ERNiCrMo-4, AWS A5.11 ENiCrMo-4Sheet: ASTM B575, ASME SB 575, ASTM B906, ASME SB 906, ISO 6208, DIN 17750, VdTüV 400/12.98Strip: ASTM B575, ASTM B906, ISO 6208, DIN 17750, VdTüV 400/12.98

Pipe: ASTM B622, ASME SB 622, ASTM B619, ASTM B775, ASTM B516, ASTM B626, ASTM B 751 & ASME SB 626; ; ASME SB 619; ASME SB 775, ISO 6207, DIN 17751, VdTüV 400/12.98,  ASTM B 829 & ASME SB 829

Rod/Bar : ASTM B 462, ASTM B574,  ASME SB 574, ISO 9723. DIN 17752. DIN 17753, DIN 17754 VdTüV 400/12.98

Nickel 200/201

Wire: BS 3072, BS 3073, BS 3074, BS 3075, BS 3076, NA11, DIN 17740, 17750, 17751, 17752, 17753, 17754, Werkstoff Nr. 2.4060, 2.4066Sheet: ASME SB-168Strip: ASME SB-160, AMS 553

Pipe: ASME SB-161, ASME SB-829, ASME SB-775, ASME SB-725, ASME SB-163,  ASME SB-730, ASME SB-751

Monel 400

Wire: BS3075NA13, ASTM B 164, ASME SB 164, ASME SB 564, AECMA PrEN 2305, SAE AMS 4675, SAE, DIN 17752, DIN 17753, VdTÜV 263, QQ-N-28Sheet: SAE AMS 4544, DIN 17750, QQ-N-28Strip: BS3072NA13, BS3073NA13, ASTM B 127, ASME SB 127

Pipe: BS3074NA13, ASTM B 163, ASTM B 165, ASTM B 725, ASTM B 730, ASTM B 751, ASTM B 775, ASTM B 829, ASME SB 163, ASME SB 165, ASME SB 725, ASME SB 730, ASME SB 751, ASME SB 775, ASME SB 829, SAE AMS 4574, DIN 1775, VdTÜV 263

Rod: BS3076NA13, ASTM B 564, AMS 4730, SAE AMS 4731, DIN 17754

Monel K-500

Wire:  ASTM B164, QQ-N-281, BS3075NA18, ASTM B 865, DIN 17753, ASME Code Case 1192, AWS A5.14 ERNiCu-7. AWS A5.11 ENiCu-7, AMS 4675, AMS 4730, AMS 4731, VdTUV 263Sheet: BS3072NA1, QQ-N-286, ISO 6208, ASTM B127, AMS 4544Strip: BS3073NA18, DIN 17750, BS 3072NA1, BS 3073NA13, QQ-N-281

Rod: BS3076NA18, DIN 17752,
DIN 17754, QQ-N-286, SAE AMS 4676, ISO 9723, ISO 9724, ISO 9725

Pipe: ASTM B165, ASTM B829, ASTM B775, ASTM B725, ASTM B163, ASTM B730, ASTM B751, ams 4574, din 17752, VdTUV 2635

Inconel 600

Wire: ASTM B 166/ASME SB 166, ASTM B 564/ASME SB 564Rod, Bar: ASTM B 166/ASME SB 166, ASTM B 564/ASME SB 564, ASME Code Cases 1827 and N-253, SAE/AMS 5665 and 5687, BS 3075NA14 and 3076NA14,DIN 17752, 17753 and 17754, ISO 9723, 9724, and 9725, MIL-DTL-23229, QQ-W-390.Plate/Sheet/Strip: SAE/AMS 5540, BS 3072NA14 and 3073NA14, DIN 17750,ASTM B 906, ASME SB 906, ASME Code Cases 1827 and N-253,ASTM B 168, ASME SB 168, ISO 6208, EN 10095, MIL-DTL-23228

Pipe/Tube: ASME Code Cases 1827, N-20, N-253, and N-576, SAE/AMS 5580,DIN 17751, ISO 6207, MIL-DTL-23227,ASTM B 517/ASME SB 517, ASTM B 751/ASME SB 751, ASTM B 775, ASME SB 775, ASTM B 829/ASME SB 829,ASTM B 167, ASME SB 167, ASTM B 163, ASME SB 163,  ASTM B 516, ASME SB 516

Others: ASTM B 366, ASME SB 366, DIN 17742, ISO 4955A, AFNOR NC15Fe

Inconel 625

Wire: AMS 5837, ISO 9724, DIN 17753 Rod/Bar: ASTM B 446, ASME SB 466, ISO 9723, VdTUV 499, BS 3076 NA21, EN 10095, DIN 17752, SME Code Case 1935,ASTM B 446, ASME SB 466, AMS 5666, ISO 9723, VdTUV 499, BS 3076 NA21, EN 10095, DIN 17752, ASME Code Case 1935 Sheet/Plate/Strip: ASTM B 443, ASME SB 443, AMS 5599, AMS 5869, MAM 5599, ISO 6208, VdTUV 499,  BS 3072 NA21, EN 10095, DIN 17750, ASME Code Case 1935

Pipe/Tube: ASTM B444, ASTM B829, ASME SB 444, ASME SB 829,  BS3074 NA21,ASTM B705, ASTM B775, ASME SB 705, ASME SB 775,  ASTM B444, ASTM B829,  AMS 5581, BS3074 NA21, ASTM B704, ASTM B751, ASME SB 704,VdTUV 499, ISO 6207, DIN 17751, ASME Code Case 1935

Others: W. Nr 2.4856, ISO NW6625, NACE MR-01-75

High Temperature Alloys

Inconel 600

Specification already mentioned above

Inconel 625

Specification already mentioned above

Inconel 601

Wire: ASTM B 166/ASME SB 166, DIN 17753Rod/Bar: ASTM B 166/ASME SB 166, DIN 17752, EN10095 ISO 9723, ISO 9724, ISO 9725Sheet/Strip/Plate: ASTM B 168/ ASME SB 168,ASTM B 168/ ASME SB 168, DIN 17750, EN10095, ISO 6208

Pipe/Tube: ASTM B 167/ASME SB 167,ASTM B 775/ASME SB 775, ASTM B 751/ASME SB 751, ASTM B 829/ASME SB 829, DIN 17751, ISO 6207

Others: ASME Code Case 1500, DIN 17742, ISO NW6601

Inconel 617

Wire: ASTM B 166, WS 2.4663a, ISO 9724, DIN 17753Rod/Bar: ASTM B 166, ASME SB-166, SAE AMS 5887,DIN 17752Sheet/Strip/Plate: VdTÜV 485 , AMS 5888,ASTM B 168; ASME SB 168,AMS 5889, ISO 6208, DIN 17750

Pipe/Tube:  ISO 6207, ASTM B 546; ASME SB 546,DIN 17751

Inconel 718

Wire: ASTM B 637, ASME SB 637, SAE AMS 5662, SAE AMS 5663, , AECMA PrEN 2404, AECMA PrEN 2405, AECMA PrEN 2952, AECMA PrEN 2961, AECMA PrEN 3219, AECMA PrEN 3666Rod/Bar: ISO 9723, ISO 9724, ISO 9725, DIN 17752-17754, ASME Code Case 2206, ASME Code Case 2222, SAE AMS 5664, SAE AMS 5832, SAE AMS 5914, SAE AMS 5962, ASME Code Case 1993Sheet/Strip/Plate: ASTM B 670, ASTM B 906, ASME SB 670, AECMA PrEN 2407,  ASME SB 670, ASME SB 906,AECMA PrEN 2408, ISO 6208, DIN 17750,SAE AMS 5596, SAE AMS 5597, SAE AMS 5950

Pipe/Tube: SAE AMS 5589, SAE AMS 5590, ASME Code Case N-253, DIN 17751,SAE AMS 5589, SAE AMS 5590, ASME Code Case N-253, DIN 17751

Other: ASME Code Case N-62, ASME Code Case N- 208, DIN 17744

Inconel X750

Wire: BS HR 505, AMS 5698, AMS 5699Rod/Bar: ASTM B 637, ASME SB 637, ISO 9723, ISO9724, ISO9725, AMS 5667, AMS 5668, AMS 5669, AMS 5670, AMS 5671, AMS 5747, EN10269Plate, Sheet, Strip:ISO 6208, AMS 5542 and AMS 5598

Other: W.Nr 2.4669

Hastelloy X

Wire: ASME SB-572, AMS 5754, AMS 5798Rod: ASME SB 572, AMS 5754, AMS 5798 Pipe: ASME SB-622, AMSE SB 829, ASME SB-619, ASME SB-775, ASTM B626, ASME SB-626, ASME SB-751, ASME SB-622, AMS 5587

Sheet/Strip: ASME SB-435, AMS 5536, ASME SB 425

Incoloy 800/800H/800HT

Wire: ASTM B 408, ASME SB 408, ISO 9723, BS 3076NA15, ISO 9724, BS 3075NA15,AMS 5766Rod/Bar: DIN 17460, EN 10095, AMS 5766,ISO 9723Plate, Sheet, Strip: AMS 5871, ASTM A 240/A 480, ASME SA 240/SA 480, ASTM B 409/B 906, ASME SB 409/SB 906, BS 3072NA15, DIN 17460, EN 10028-7, EN 10095

Pipe/Tube: ASTM B 407/B 829, ASME SB 407/SB 829 (Seamless Pipe), BS 3074NA15 (Seamless Pipe), DIN 17459, ASTM B 514/B 775 & ASME SB 514/SB 775, ASME N-20, BS 3074NA15,ASTM B 163, ASME SB 163 ASTM B 515/B 751, ASME SB 515/SB 751, BS 3074NA15, ISO 6207, DIN 17459, ASTM B 515/B 751,  ASME Code Case 1325, VdTÜV 412, ISO 6207

Other: ASME Code Cases N201 & N254, ISO 4955A, NACE MR-01-75, AFNOR Z5 NC 35-20, ASME Code Case 1325, SEW 470, VdTUV 412 and 434

Incoloy 825

Wire: ASTM B 425, DIN 17752, ASME Code Case N-572Rod/Bar:  DIN 17753, DIN 17754, VdTÜV 432, ISO 9723, ISO 9724, ISO 9725,BS 3076NA16, , ASTM B 564, ASME SB 425, ASME SB 564,Plate/Sheet/Strip: BS 3072NA16, BS 3073NA16, ASTM B 424, ASTM B 906, ASME SB 424, ASME SB 906, DIN 17750, VdTÜV 432, ISO 6208

Pipe/Tube: BS 3074NA16, ASTM B 163, ASTM B 423, ASTM B 704, ASTM B 705, ASTM B 751, ASTM B 775, ASTM B 829, ASME SB 163, ASME SB 423, ASME SB 704, ASME SB 705, ASME SB 751, ASME SB 775, ASME SB 829, ASME Code Case 1936, DIN 17751, VdTÜV 432, ISO 6207

Other: ASTM B 366, ASME SB 366, DIN 17744

Nimonic 75

Wire: BS HR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725, MSRR 7004Sheet/Strip: BS HR 203, AECMA PrEN2302, AECMA PrEN2411, ISO 6208, MSRR 7104, DIN 17750, AECMA PrEN2293

Nimonic 80A

Wire: BS 3076 HR1, ASTM B 637, AECMA PrEn2188, AECMA PrEn2189, AECMA PrEn 2190, AECMA PrEn 2396, AECMA PrEn2397, AIR 9165-37, BS HR 601, BS HR1, DIN 17742, AFNOR NC 20TA, UNS N07080, Werkstoff Nr 2.4952, Werkstoff Nr 2.4631, NIMONIC 80a (trademark), MSRR 7095 and MSRR 7011Sheet/Strip: BS HR 201, AECMA PrEn2191, MSRR 7013, HR201, HR401, HR601, NA20, VAT80A

Electric Resistance Heating Alloys

Nichrome 60 Heating alloy

ASTM-B-344, ASTM B267

Nichrome 80

ASTM-B-344, ASTM B267, DIN 2.4639, DIN 2.4869, UNS N06003

FeCrAl Heating Alloy

ASTM B603, DIN 17470, JIS C2520, GB/T1234

Electronic Alloys

Nilo 36

Wire: SEW 38, MIL-S-16598Sheet/Strip: ASTM B 388,ASTM B 753, DIN 171, MIL-I-23011 CL 7,SEW 385All Forms: ASTM F-1684, MIL 1-23011 CL 7, AMS 1-230 11 CL 7

Composition: AFNOR NF A54-301

Nilo 42

Wire: ASTM F29, ASTM F 30Sheet/Strip: SEW 385, ASTM F 30, B753Composition: DIN 17745, AFNOR NF A54-301

All Forms: MIL 1-23011 CL 7, AMS 1-230 11 CL 7

Nilo 48

Wire: ASTM F30, DIN 17745Strip/Sheet: ASTM F30Composition: DIN 17745, AFNOR NF A54-301

Nilo 52

Wire: ASTM F30Sheet/Strip: ASTM F30All Forms: AMS 123011 CL 2, MIL 123011CL2

 Copper-Nickel alloy 70/30

ASME SB111, SB171, SB359, SB395, SB466, SB467, SB543, ASTM B111, B122, B151, B171, B359, B395, , B 402, B432, B 466, B467, B543, B552, B608, F467, F468, DIN 2.0882, MIL C-15726, T-15005, T-16420, T-22214, SAE J461, J463, ASTM 715, DIN 17664, 17670, 1762, 1785, 17671

 Stainless Steel 316/316l

W.Nr 1.4404, Euronorm X1 CrNiMo 17 12 2 / X3 CrNiMo 17 12 2, AFNOR Z7CND 18-12-03, AFNOR: Z 6 CND 17-11 / Z 2 CND 17-12, AISI 316, AMS 5524, AMS 5573, AMS 5648, AMS 5690,  AMS 5696, ASTM A167, ASTM A182, ASTM A193(B8M,MA,M2 & M3), ASTM A194 (316, 8M, 8MA), ASTM A213, ASTM A240, ASTM A249, ASTM A269, ASTM A270, ASTM A271, ASTM A276, ASTM A312, ASTM A313, ASTM A314,  ASTM A320 (316,B8M,B8MA), ASTM A336, ASTM A358, ASTM A368, ASTM A376, ASTM A403, ASTM A409, ASTM A430, ASTM A473, ASTM A478, ASTM A479, ASTM A492, ASTM A493, ASTM A511, ASTM A554, ASTM A580, ASTM A632, ASTM A666, ASTM A688, ASTM A771, ASTM A813, ASTM A814, ASTM A826, ASTM F138, DIN 1.4401, DIN 1.4436, MIL S-5059, MIL S-7720, QQ S763, QQ S766, UNS S31600

 Mumetal

MIL-N-14411 C (MR), ASTM A-753-78

Inconel 600

Specification already mentioned above

Inconel 601

Specification already mentioned above

Inconel 625

Specification already mentioned above

Inconel X750

Specification already mentioned above

Monel 400

Specification already mentioned above

Monel K500

Specification already mentioned above

Nickel 200/201

Specification already mentioned above

Austenitic/Ferritic Stainless Steels

Duplex 2205

ASTM A 182, ASTM A 240,  ASTM A 276, ASTM A479, A 789, A 790, A 815 UNS S31803, S32205, NACE MR0175, 318S13, EURONORM: 1.4462 X2CrNiMoN 22.5.3, AFNOR: Z3 CrNi 22.05 AZ, DIN: W.Nr 1.4462, ASME: A240, SS 2377, SUS 329J3L, A 22Cr-3Mo Stainless Steel, A790, A789, A240, A276, A182, A240M

Duplex 2507

Wire: ASTM A 164,  ASME SA 164Pipe/Tubes: ASTM A 789 / 790, ASME SA 789 / 790, ASTMA 789 / 790 , ASME SA 789 / 790Sheet/Strip: ASTM A 240, ASME SA 240

Rod/Bar: ASTM A276 / 479, ASME SA 276 / 479

 Stainless steel 310/310S

DIN 1.4845, ASTM A 240, A 276, A 312, W. Nr. 1.4845, AISI 310, AMS 5577, AMS 5651, ASTM A167, ASTM A182, ASTM A213, ASTM A249, ASTM A276, ASTM A314, ASTM A358, ASTM A403, ASTM A409, ASTM A473, ASTM A479, ASTM A580, ASTM A632, DIN 1.4841, QQ S763, QQ S766, UNS S31000

Steel 330        

Wire: SAE AMS 5716Sheet/Strip: ASTM B 536, ASME SB 536, SAE AMS 5592Rod/Bar: ASTM B 511, ASME SB 511, ASTM B 512, ASME SB 512

Pipe/Tube: ASTM B 535/ASME SB 535, ASTM B 546/ASME SB 546, ASTM B 710/ASME SB 710, ASTM B 739/ASME SB 739, ASTM B 829/ASME SB 829      

SS 904l

AFNOR Z2CNDU 25-20, VLX904, AL 904L, Cronifer 1925 LC, EN number 1.4539, EN name X1NiCrMoCu25-20-5, W.Nr. 1.4539, DIN X1 NiCrMoCu25 20 5, BS 904S13, ASTM B625, ASTM B649, ASTM B673, ASTM B674, ASTM B677, DIN 1.4539, ASTM A213, ASTM A269, ASTM A312, BS EN 10216 pt.5

 Other Superalloys

Incoloy A286

Wire: ASTM A 638, ASME SA 638, SAE AMS 5726, SAE AMS 5731, AMS 5895, BS HR 51, BS HR 52Rod/Bar: SAE AMS 5732, SAE AMS 5734, SAE AMS 5737, SAE AECMA PrEn2171, AECMA PrEN2119, AECMA PrEN2172, AECMA PrEN2173, AECMA PrEN2174, AECMA PrEN2303,AECMA PrEN2304, AECMA PrEN2398, AECMA PrEN2399, AECMA PrEN3510Plate/Sheet/Strip: SAE AMS 5525, SAE AMS 5858, AECMA PrEN2175, AECMA PrEN2417, GE B50T1181C, GE B50T12A&C, GE B50T81A&C 

Pipe/Tube: SAE AMS 5731, SAE AMS 5732, SAE AMS 5734, SAE AMS 5737, SAE AMS 5895

Other: ASTM A 453, SAE AMS 7235, BS HR 650, ASME SA 453

 Hastelloy B3

Wire: ASME SB-335, A5.14 ERNiMo-7, ASME SFA 5.11(ENiMo-7) AWS A5.11 (ENiMo-7)Sheet/Plate: ASME SB-333, ASTM B333Pipe/Tube: ASME SB-622, ASME SB-619, ASME SB-626, ASTM B622, CLASS I or II, ASTM B775, ASME SB775

Rod/Bar: ASME SB-335, ASME SFA 5.14(ENiMo-7),  ASTM B 335, ASTM B564, ASME SB564

Hastelloy C4

Wire: ASTM B574, ASME SB574Rod/Bar: ASTM B574, ASME SB574Pipe/Tube: ASTM B336, ASTM B619, ASTM B626, ASTM B622, ASME SB 336

Sheet/Strip: ASTM B575, ASME SB575

Hastelloy C2000

Wire: ASME SB 574/ASTM B 574, TUV Kennblatt 9679.00Sheet/Strip: ASME SB 575/ ASTM B 575Pipe/Tube: ASME SB 619/ASTM B 619, SB 622/B 622, SB 626/B 626, SB 462/B 462

Rod/Bar: ASTM B574, ASME SB 574, ASTM 472, TUV Kennblatt 9678.00

Flanges: ASME SB 462, ASTM B462, ASME B16.5

All Forms: ASME Section VIII, Div. 1 (P=43), DIN 17744 No. 2.4675, DIN NiCr23Mo16Cu, TUV Werkstoffblatt 539

Hastelloy G30

Wire: ASTM B581, DIN 2.4603, ASME SB 366Pipe/Tube: ASTM B619,  ASME SB619, ASTM B622, ASME SB622 ASTM B626, ASME SB626Rod/Bar: ASTM B581, ASME SB 581

Sheet/ Strip: ASTM B582, ASME SB 582

Copper-Nickel alloy 90/10

ASME SB111, SB171, SB359, SB395, SB466, SB467, SB543, ASTM B111, B122, B151, B171, B359, B395, B432, B466, B467, B543, B608, DIN 2.0872, MIL C-15726, T-15005, T-16420, T-22214, SAE J461, J463

Carpenter HyMu 80 (Permalloy)

ASTM A-753-78, , MIL-N-14411 B (MR), MIL N 14411C

Nimonic 90

Wire: BS HR2, HR501, HR502 and HR503; SAE AMS 5829; AECMA PrEN 2295, 2296, 2297, 2400, 2401, 2669 and 2670Sheet/Strip: BS HR202, AECMA PrEN 2298

Nickel Span C902

SAE AMS 5221, AMS 5223, AMS 5225, AMS 5210, BS 3127
Call Now Button